O-ring Material Compatibility for Chemicals Starting with D
check 430.000.000+ O-rings in stock
check Fast delivery

check Fast delivery

check 430.000.000+ O-rings in stock

O-ring Material Compatibility for Chemicals Starting with D

  • event 10-07-2026
  • schedule 13:00
  • timer 63 minuten
Home Knowledge Base Chemical Resistance Guide
O-ring Material Compatibility for Chemicals Starting with A O-ring Material Compatibility for Chemicals Starting with B O-ring Material Compatibility for Chemicals Starting with C O-ring Material Compatibility for Chemicals Starting with D O-ring Material Compatibility for Chemicals Starting with E O-ring Material Compatibility for Chemicals Starting with F O-ring Material Compatibility for Chemicals Starting with G O-ring Material Compatibility for Chemicals Starting with H O-ring Material Compatibility for Chemicals Starting with I O-ring Material Compatibility for Chemicals Starting with J O-ring Material Compatibility for Chemicals Starting with K O-ring Material Compatibility for Chemicals Starting with L O-ring Material Compatibility for Chemicals Starting with M O-ring Material Compatibility for Chemicals Starting with N O-ring Material Compatibility for Chemicals Starting with O O-ring Material Compatibility for Chemicals Starting with P O-ring Material Compatibility for Chemicals Starting with Q O-ring Material Compatibility for Chemicals Starting with R O-ring Material Compatibility for Chemicals Starting with S O-ring Material Compatibility for Chemicals Starting with T O-ring Material Compatibility for Chemicals Starting with U O-ring Material Compatibility for Chemicals Starting with V O-ring Material Compatibility for Chemicals Starting with W O-ring Material Compatibility for Chemicals Starting with X O-ring Material Compatibility for Chemicals Starting with Y O-ring Material Compatibility for Chemicals Starting with Z

Which O-ring do I need for DDT (Dichlorodiphenyltrichloroethane)?

FPM O-rings are the best option for contact with DDT (Dichlorodiphenyltrichloroethane), based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DDT (Dichlorodiphenyltrichloroethane) with a maximum swelling of less than 15%, but at a higher cost than FPM and FVMQ. HNBR and AU O-rings are less resistant to DDT (Dichlorodiphenyltrichloroethane) and should only be used after checking the application conditions. Do not use NBR, EPDM, VMQ, FEP and PTFE O-rings for DDT (Dichlorodiphenyltrichloroethane), as these materials are not recommended or have not been tested for resistance to DDT (Dichlorodiphenyltrichloroethane).



Which O-ring do I need for DECAHYDRONAPHTHALENE?

FPM O-rings are the best option for contact with DECAHYDRONAPHTHALENE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DECAHYDRONAPHTHALENE with a maximum swelling of less than 15%, but at a higher cost than FPM and FVMQ. Do not use NBR, EPDM, HNBR, VMQ, FEP, AU and PTFE O-rings for DECAHYDRONAPHTHALENE, as these materials are not recommended or have not been tested for resistance to DECAHYDRONAPHTHALENE.



Which O-ring do I need for DECALIN?

FPM O-rings are the best option for contact with DECALIN, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DECALIN with a maximum swelling of less than 15%, but at a higher cost than FPM and FVMQ. FEP O-rings are less resistant to DECALIN and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, AU and PTFE O-rings for DECALIN, as these materials are not recommended or have not been tested for resistance to DECALIN.



Which O-ring do I need for DECANE?

NBR O-rings are the best option for contact with DECANE, based on chemical resistance and relative cost. HNBR, FPM, FEP, FVMQ and FFKM O-rings offer the same chemical resistance to DECANE with a maximum swelling of less than 15%, but at a higher cost than NBR. VMQ and AU O-rings are less resistant to DECANE and should only be used after checking the application conditions. Do not use EPDM and PTFE O-rings for DECANE, as these materials are not recommended or have not been tested for resistance to DECANE.



Which O-ring do I need for DEIONIZED WATER?

FPM O-rings are the best option for contact with DEIONIZED WATER, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DEIONIZED WATER with a maximum swelling of less than 15%, but at a higher cost than FPM and FVMQ. NBR, EPDM, HNBR, VMQ and FEP O-rings are less resistant to DEIONIZED WATER and should only be used after checking the application conditions. Do not use AU and PTFE O-rings for DEIONIZED WATER, as these materials are not recommended or have not been tested for resistance to DEIONIZED WATER.



Which O-ring do I need for DELCO BRAKE FLUID?

EPDM O-rings are the best option for contact with DELCO BRAKE FLUID, based on chemical resistance and relative cost. FEP and FFKM O-rings offer the same chemical resistance to DELCO BRAKE FLUID with a maximum swelling of less than 15%, but at a higher cost than EPDM. NBR, HNBR and VMQ O-rings are less resistant to DELCO BRAKE FLUID and should only be used after checking the application conditions. Do not use FPM, FVMQ, AU and PTFE O-rings for DELCO BRAKE FLUID, as these materials are not recommended or have not been tested for resistance to DELCO BRAKE FLUID.



Which O-ring do I need for DELTA H?

PTFE O-rings are the best option for contact with DELTA H, based on chemical resistance and relative cost. These materials offer chemical resistance to DELTA H with a maximum swelling of less than 15%. FPM and FFKM O-rings are less resistant to DELTA H and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FEP, FVMQ and AU O-rings for DELTA H, as these materials are not recommended or have not been tested for resistance to DELTA H.



Which O-ring do I need for DELVAC 1100, 1110, 1120, 1130?

NBR O-rings are the best option for contact with DELVAC 1100, 1110, 1120, 1130, based on chemical resistance and relative cost. HNBR, VMQ, FPM, FEP and FFKM O-rings offer the same chemical resistance to DELVAC 1100, 1110, 1120, 1130 with a maximum swelling of less than 15%, but at a higher cost than NBR. Do not use EPDM, FVMQ, AU and PTFE O-rings for DELVAC 1100, 1110, 1120, 1130, as these materials are not recommended or have not been tested for resistance to DELVAC 1100, 1110, 1120, 1130.



Which O-ring do I need for DENATURED ALCOHOL?

NBR O-rings and EPDM O-rings are the best option for contact with DENATURED ALCOHOL, based on chemical resistance and relative cost. HNBR, VMQ, FPM, FEP, FVMQ, PTFE and FFKM O-rings offer the same chemical resistance to DENATURED ALCOHOL with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. Do not use AU O-rings for DENATURED ALCOHOL, as these materials are not recommended or have not been tested for resistance to DENATURED ALCOHOL.



Which O-ring do I need for DESMODUR?

No rating 1 O-ring material is listed for DESMODUR in this chemical resistance guide. AU O-rings are less resistant to DESMODUR and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FPM, FEP, FVMQ, PTFE and FFKM O-rings for DESMODUR, as these materials are not recommended or have not been tested for resistance to DESMODUR.



Which O-ring do I need for DESMOPHEN 2000?

NBR O-rings are the best option for contact with DESMOPHEN 2000, based on chemical resistance and relative cost. HNBR and PTFE O-rings offer the same chemical resistance to DESMOPHEN 2000 with a maximum swelling of less than 15%, but at a higher cost than NBR. Do not use EPDM, VMQ, FPM, FEP, FVMQ, AU and FFKM O-rings for DESMOPHEN 2000, as these materials are not recommended or have not been tested for resistance to DESMOPHEN 2000.



Which O-ring do I need for DETERGENT SOLUTIONS?

NBR O-rings and EPDM O-rings are the best option for contact with DETERGENT SOLUTIONS, based on chemical resistance and relative cost. HNBR, VMQ, FPM, FEP, FVMQ, PTFE and FFKM O-rings offer the same chemical resistance to DETERGENT SOLUTIONS with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. Do not use AU O-rings for DETERGENT SOLUTIONS, as these materials are not recommended or have not been tested for resistance to DETERGENT SOLUTIONS.



Which O-ring do I need for DETERGENTS?

NBR O-rings and EPDM O-rings are the best option for contact with DETERGENTS, based on chemical resistance and relative cost. HNBR and PTFE O-rings offer the same chemical resistance to DETERGENTS with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. FPM and FFKM O-rings are less resistant to DETERGENTS and should only be used after checking the application conditions. Do not use VMQ, FEP, FVMQ and AU O-rings for DETERGENTS, as these materials are not recommended or have not been tested for resistance to DETERGENTS.



Which O-ring do I need for DEVELOPING FLUIDS?

NBR O-rings are the best option for contact with DEVELOPING FLUIDS, based on chemical resistance and relative cost. HNBR, VMQ, FPM, FEP, FVMQ and FFKM O-rings offer the same chemical resistance to DEVELOPING FLUIDS with a maximum swelling of less than 15%, but at a higher cost than NBR. EPDM O-rings are less resistant to DEVELOPING FLUIDS and should only be used after checking the application conditions. Do not use AU and PTFE O-rings for DEVELOPING FLUIDS, as these materials are not recommended or have not been tested for resistance to DEVELOPING FLUIDS.



Which O-ring do I need for DEXRON?

NBR O-rings are the best option for contact with DEXRON, based on chemical resistance and relative cost. HNBR, FPM and FFKM O-rings offer the same chemical resistance to DEXRON with a maximum swelling of less than 15%, but at a higher cost than NBR. FEP, FVMQ and AU O-rings are less resistant to DEXRON and should only be used after checking the application conditions. Do not use EPDM, VMQ and PTFE O-rings for DEXRON, as these materials are not recommended or have not been tested for resistance to DEXRON.



Which O-ring do I need for DEXTRIN?

NBR O-rings and EPDM O-rings are the best option for contact with DEXTRIN, based on chemical resistance and relative cost. HNBR, VMQ, FPM, FVMQ, PTFE and FFKM O-rings offer the same chemical resistance to DEXTRIN with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. Do not use FEP and AU O-rings for DEXTRIN, as these materials are not recommended or have not been tested for resistance to DEXTRIN.



Which O-ring do I need for DEXTRO LACTIC ACID?

EPDM O-rings are the best option for contact with DEXTRO LACTIC ACID, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DEXTRO LACTIC ACID with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR, HNBR and FPM O-rings are less resistant to DEXTRO LACTIC ACID and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DEXTRO LACTIC ACID, as these materials are not recommended or have not been tested for resistance to DEXTRO LACTIC ACID.



Which O-ring do I need for DEXTRON?

NBR O-rings are the best option for contact with DEXTRON, based on chemical resistance and relative cost. HNBR, FPM, FEP and FFKM O-rings offer the same chemical resistance to DEXTRON with a maximum swelling of less than 15%, but at a higher cost than NBR. FVMQ O-rings are less resistant to DEXTRON and should only be used after checking the application conditions. Do not use EPDM, VMQ, AU and PTFE O-rings for DEXTRON, as these materials are not recommended or have not been tested for resistance to DEXTRON.



Which O-ring do I need for DEXTROSE?

EPDM O-rings are the best option for contact with DEXTROSE, based on chemical resistance and relative cost. FPM, FVMQ and FFKM O-rings offer the same chemical resistance to DEXTROSE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR and HNBR O-rings are less resistant to DEXTROSE and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DEXTROSE, as these materials are not recommended or have not been tested for resistance to DEXTROSE.



Which O-ring do I need for DIACETONE?

EPDM O-rings are the best option for contact with DIACETONE, based on chemical resistance and relative cost. PTFE and FFKM O-rings offer the same chemical resistance to DIACETONE with a maximum swelling of less than 15%, but at a higher cost than EPDM. FEP O-rings are less resistant to DIACETONE and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FPM, FVMQ and AU O-rings for DIACETONE, as these materials are not recommended or have not been tested for resistance to DIACETONE.



Which O-ring do I need for DIACETONE ALCOHOL?

EPDM O-rings are the best option for contact with DIACETONE ALCOHOL, based on chemical resistance and relative cost. PTFE and FFKM O-rings offer the same chemical resistance to DIACETONE ALCOHOL with a maximum swelling of less than 15%, but at a higher cost than EPDM. Do not use NBR, HNBR, VMQ, FPM, FEP, FVMQ and AU O-rings for DIACETONE ALCOHOL, as these materials are not recommended or have not been tested for resistance to DIACETONE ALCOHOL.



Which O-ring do I need for DIALKYL SULFATES?

EPDM O-rings are the best option for contact with DIALKYL SULFATES, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIALKYL SULFATES with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR, HNBR and FPM O-rings are less resistant to DIALKYL SULFATES and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DIALKYL SULFATES, as these materials are not recommended or have not been tested for resistance to DIALKYL SULFATES.



Which O-ring do I need for DIAMYLAMINE?

NBR O-rings are the best option for contact with DIAMYLAMINE, based on chemical resistance and relative cost. HNBR, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DIAMYLAMINE with a maximum swelling of less than 15%, but at a higher cost than NBR. VMQ O-rings are less resistant to DIAMYLAMINE and should only be used after checking the application conditions. Do not use EPDM, FPM, FEP and PTFE O-rings for DIAMYLAMINE, as these materials are not recommended or have not been tested for resistance to DIAMYLAMINE.



Which O-ring do I need for DIAZINON?

FFKM O-rings are the best option for contact with DIAZINON, based on chemical resistance and relative cost. These materials offer chemical resistance to DIAZINON with a maximum swelling of less than 15%. FPM, FVMQ, NBR and HNBR O-rings are less resistant to DIAZINON and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP, AU and PTFE O-rings for DIAZINON, as these materials are not recommended or have not been tested for resistance to DIAZINON.



Which O-ring do I need for DIBENZYL?

FFKM O-rings are the best option for contact with DIBENZYL, based on chemical resistance and relative cost. These materials offer chemical resistance to DIBENZYL with a maximum swelling of less than 15%. NBR, HNBR, FPM, FVMQ and AU O-rings are less resistant to DIBENZYL and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIBENZYL, as these materials are not recommended or have not been tested for resistance to DIBENZYL.



Which O-ring do I need for DIBENZYL ETHER?

PTFE O-rings are the best option for contact with DIBENZYL ETHER, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIBENZYL ETHER with a maximum swelling of less than 15%, but at a higher cost than PTFE. EPDM, AU and FEP O-rings are less resistant to DIBENZYL ETHER and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FPM and FVMQ O-rings for DIBENZYL ETHER, as these materials are not recommended or have not been tested for resistance to DIBENZYL ETHER.



Which O-ring do I need for DIBENZYL SEBACATE?

FEP O-rings are the best option for contact with DIBENZYL SEBACATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIBENZYL SEBACATE with a maximum swelling of less than 15%, but at a higher cost than FEP. EPDM, FPM, AU, VMQ and FVMQ O-rings are less resistant to DIBENZYL SEBACATE and should only be used after checking the application conditions. Do not use NBR, HNBR and PTFE O-rings for DIBENZYL SEBACATE, as these materials are not recommended or have not been tested for resistance to DIBENZYL SEBACATE.



Which O-ring do I need for DIBROMODIFLUOROMETHANE?

FFKM O-rings are the best option for contact with DIBROMODIFLUOROMETHANE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIBROMODIFLUOROMETHANE with a maximum swelling of less than 15%. EPDM O-rings are less resistant to DIBROMODIFLUOROMETHANE and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FPM, FEP, FVMQ, AU and PTFE O-rings for DIBROMODIFLUOROMETHANE, as these materials are not recommended or have not been tested for resistance to DIBROMODIFLUOROMETHANE.



Which O-ring do I need for DIBROMOETHANE?

FPM O-rings are the best option for contact with DIBROMOETHANE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIBROMOETHANE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIBROMOETHANE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIBROMOETHANE, as these materials are not recommended or have not been tested for resistance to DIBROMOETHANE.



Which O-ring do I need for DIBROMOETHYLBENZENE?

FFKM O-rings are the best option for contact with DIBROMOETHYLBENZENE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIBROMOETHYLBENZENE with a maximum swelling of less than 15%. FPM and FVMQ O-rings are less resistant to DIBROMOETHYLBENZENE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FEP, AU and PTFE O-rings for DIBROMOETHYLBENZENE, as these materials are not recommended or have not been tested for resistance to DIBROMOETHYLBENZENE.



Which O-ring do I need for DIBROMOTETRAFLUOROETHANE?

No rating 1 O-ring material is listed for DIBROMOTETRAFLUOROETHANE in this chemical resistance guide. NBR, FPM and FFKM O-rings are less resistant to DIBROMOTETRAFLUOROETHANE and should only be used after checking the application conditions. Do not use EPDM, HNBR, VMQ, FEP, FVMQ, AU and PTFE O-rings for DIBROMOTETRAFLUOROETHANE, as these materials are not recommended or have not been tested for resistance to DIBROMOTETRAFLUOROETHANE.



Which O-ring do I need for DIBUTYL CELLOSOLVE ADIPATE?

EPDM O-rings are the best option for contact with DIBUTYL CELLOSOLVE ADIPATE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIBUTYL CELLOSOLVE ADIPATE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR, HNBR and FPM O-rings are less resistant to DIBUTYL CELLOSOLVE ADIPATE and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DIBUTYL CELLOSOLVE ADIPATE, as these materials are not recommended or have not been tested for resistance to DIBUTYL CELLOSOLVE ADIPATE.



Which O-ring do I need for DIBUTYL ETHER?

PTFE O-rings are the best option for contact with DIBUTYL ETHER, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIBUTYL ETHER with a maximum swelling of less than 15%, but at a higher cost than PTFE. AU, EPDM, FPM and FVMQ O-rings are less resistant to DIBUTYL ETHER and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ and FEP O-rings for DIBUTYL ETHER, as these materials are not recommended or have not been tested for resistance to DIBUTYL ETHER.



Which O-ring do I need for DIBUTYL METHYLENEDITHIO GLYCOLATE?

FPM O-rings are the best option for contact with DIBUTYL METHYLENEDITHIO GLYCOLATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIBUTYL METHYLENEDITHIO GLYCOLATE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIBUTYL METHYLENEDITHIO GLYCOLATE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIBUTYL METHYLENEDITHIO GLYCOLATE, as these materials are not recommended or have not been tested for resistance to DIBUTYL METHYLENEDITHIO GLYCOLATE.



Which O-ring do I need for DIBUTYL PHTHALATE?

PTFE O-rings are the best option for contact with DIBUTYL PHTHALATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIBUTYL PHTHALATE with a maximum swelling of less than 15%, but at a higher cost than PTFE. EPDM, VMQ, FEP, FPM, FVMQ and AU O-rings are less resistant to DIBUTYL PHTHALATE and should only be used after checking the application conditions. Do not use NBR and HNBR O-rings for DIBUTYL PHTHALATE, as these materials are not recommended or have not been tested for resistance to DIBUTYL PHTHALATE.



Which O-ring do I need for DIBUTYL SEBACATE?

PTFE O-rings are the best option for contact with DIBUTYL SEBACATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIBUTYL SEBACATE with a maximum swelling of less than 15%, but at a higher cost than PTFE. EPDM, VMQ, FEP and FVMQ O-rings are less resistant to DIBUTYL SEBACATE and should only be used after checking the application conditions. Do not use NBR, HNBR, FPM and AU O-rings for DIBUTYL SEBACATE, as these materials are not recommended or have not been tested for resistance to DIBUTYL SEBACATE.



Which O-ring do I need for DIBUTYL THIOGLYCOLATE?

FPM O-rings are the best option for contact with DIBUTYL THIOGLYCOLATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIBUTYL THIOGLYCOLATE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIBUTYL THIOGLYCOLATE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIBUTYL THIOGLYCOLATE, as these materials are not recommended or have not been tested for resistance to DIBUTYL THIOGLYCOLATE.



Which O-ring do I need for DIBUTYL THIOUREA?

FPM O-rings are the best option for contact with DIBUTYL THIOUREA, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIBUTYL THIOUREA with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIBUTYL THIOUREA and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIBUTYL THIOUREA, as these materials are not recommended or have not been tested for resistance to DIBUTYL THIOUREA.



Which O-ring do I need for DIBUTYLAMINE?

FFKM O-rings are the best option for contact with DIBUTYLAMINE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIBUTYLAMINE with a maximum swelling of less than 15%. FEP and VMQ O-rings are less resistant to DIBUTYLAMINE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, FPM, FVMQ, AU and PTFE O-rings for DIBUTYLAMINE, as these materials are not recommended or have not been tested for resistance to DIBUTYLAMINE.



Which O-ring do I need for DICAPRYL PHTHALATE?

FFKM O-rings are the best option for contact with DICAPRYL PHTHALATE, based on chemical resistance and relative cost. These materials offer chemical resistance to DICAPRYL PHTHALATE with a maximum swelling of less than 15%. EPDM, FPM, FVMQ and VMQ O-rings are less resistant to DICAPRYL PHTHALATE and should only be used after checking the application conditions. Do not use NBR, HNBR, FEP, AU and PTFE O-rings for DICAPRYL PHTHALATE, as these materials are not recommended or have not been tested for resistance to DICAPRYL PHTHALATE.



Which O-ring do I need for DICHCLOROBUTANE?

FPM O-rings and FEP O-rings are the best option for contact with DICHCLOROBUTANE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHCLOROBUTANE with a maximum swelling of less than 15%, but at a higher cost than FPM and FEP. NBR and HNBR O-rings are less resistant to DICHCLOROBUTANE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FVMQ, AU and PTFE O-rings for DICHCLOROBUTANE, as these materials are not recommended or have not been tested for resistance to DICHCLOROBUTANE.



Which O-ring do I need for DICHLORACETIC ACID?

EPDM O-rings are the best option for contact with DICHLORACETIC ACID, based on chemical resistance and relative cost. PTFE O-rings offer the same chemical resistance to DICHLORACETIC ACID with a maximum swelling of less than 15%, but at a higher cost than EPDM. FFKM O-rings are less resistant to DICHLORACETIC ACID and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FPM, FEP, FVMQ and AU O-rings for DICHLORACETIC ACID, as these materials are not recommended or have not been tested for resistance to DICHLORACETIC ACID.



Which O-ring do I need for DICHLORETHANE?

PTFE O-rings are the best option for contact with DICHLORETHANE, based on chemical resistance and relative cost. These materials offer chemical resistance to DICHLORETHANE with a maximum swelling of less than 15%. FPM and FFKM O-rings are less resistant to DICHLORETHANE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FEP, FVMQ and AU O-rings for DICHLORETHANE, as these materials are not recommended or have not been tested for resistance to DICHLORETHANE.



Which O-ring do I need for DICHLORETHYLENE?

PTFE O-rings are the best option for contact with DICHLORETHYLENE, based on chemical resistance and relative cost. These materials offer chemical resistance to DICHLORETHYLENE with a maximum swelling of less than 15%. FPM and FFKM O-rings are less resistant to DICHLORETHYLENE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FEP, FVMQ and AU O-rings for DICHLORETHYLENE, as these materials are not recommended or have not been tested for resistance to DICHLORETHYLENE.



Which O-ring do I need for DICHLOROACETIC ACID?

FPM O-rings are the best option for contact with DICHLOROACETIC ACID, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHLOROACETIC ACID with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DICHLOROACETIC ACID and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DICHLOROACETIC ACID, as these materials are not recommended or have not been tested for resistance to DICHLOROACETIC ACID.



Which O-ring do I need for DICHLOROANILINE?

EPDM O-rings are the best option for contact with DICHLOROANILINE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DICHLOROANILINE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR and HNBR O-rings are less resistant to DICHLOROANILINE and should only be used after checking the application conditions. Do not use FPM, FEP, AU and PTFE O-rings for DICHLOROANILINE, as these materials are not recommended or have not been tested for resistance to DICHLOROANILINE.



Which O-ring do I need for DICHLOROBENZENE?

FPM O-rings and PTFE O-rings are the best option for contact with DICHLOROBENZENE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHLOROBENZENE with a maximum swelling of less than 15%, but at a higher cost than FPM and PTFE. FVMQ and FEP O-rings are less resistant to DICHLOROBENZENE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ and AU O-rings for DICHLOROBENZENE, as these materials are not recommended or have not been tested for resistance to DICHLOROBENZENE.



Which O-ring do I need for DICHLOROBUTANE?

FPM O-rings, FEP O-rings and PTFE O-rings are the best option for contact with DICHLOROBUTANE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHLOROBUTANE with a maximum swelling of less than 15%, but at a higher cost than FPM, FEP and PTFE. NBR, HNBR and FVMQ O-rings are less resistant to DICHLOROBUTANE and should only be used after checking the application conditions. Do not use EPDM, VMQ and AU O-rings for DICHLOROBUTANE, as these materials are not recommended or have not been tested for resistance to DICHLOROBUTANE.



Which O-ring do I need for DICHLOROBUTENE?

PTFE O-rings are the best option for contact with DICHLOROBUTENE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHLOROBUTENE with a maximum swelling of less than 15%, but at a higher cost than PTFE. FPM, FVMQ and AU O-rings are less resistant to DICHLOROBUTENE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ and FEP O-rings for DICHLOROBUTENE, as these materials are not recommended or have not been tested for resistance to DICHLOROBUTENE.



Which O-ring do I need for DICHLORODIETHYL SULFIDE?

EPDM O-rings are the best option for contact with DICHLORODIETHYL SULFIDE, based on chemical resistance and relative cost. VMQ and FFKM O-rings offer the same chemical resistance to DICHLORODIETHYL SULFIDE with a maximum swelling of less than 15%, but at a higher cost than EPDM. Do not use NBR, HNBR, FPM, FEP, FVMQ, AU and PTFE O-rings for DICHLORODIETHYL SULFIDE, as these materials are not recommended or have not been tested for resistance to DICHLORODIETHYL SULFIDE.



Which O-ring do I need for DICHLORODIPHENYLDICHLOROETHANE?

FPM O-rings are the best option for contact with DICHLORODIPHENYLDICHLOROETHANE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHLORODIPHENYLDICHLOROETHANE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DICHLORODIPHENYLDICHLOROETHANE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DICHLORODIPHENYLDICHLOROETHANE, as these materials are not recommended or have not been tested for resistance to DICHLORODIPHENYLDICHLOROETHANE.



Which O-ring do I need for DICHLOROETHANE?

FPM O-rings are the best option for contact with DICHLOROETHANE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHLOROETHANE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DICHLOROETHANE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DICHLOROETHANE, as these materials are not recommended or have not been tested for resistance to DICHLOROETHANE.



Which O-ring do I need for DICHLOROETHYLENE?

FFKM O-rings are the best option for contact with DICHLOROETHYLENE, based on chemical resistance and relative cost. These materials offer chemical resistance to DICHLOROETHYLENE with a maximum swelling of less than 15%. NBR, HNBR, FPM, FVMQ and AU O-rings are less resistant to DICHLOROETHYLENE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DICHLOROETHYLENE, as these materials are not recommended or have not been tested for resistance to DICHLOROETHYLENE.



Which O-ring do I need for DICHLOROHYDRIN?

EPDM O-rings are the best option for contact with DICHLOROHYDRIN, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DICHLOROHYDRIN with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR, HNBR and FPM O-rings are less resistant to DICHLOROHYDRIN and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DICHLOROHYDRIN, as these materials are not recommended or have not been tested for resistance to DICHLOROHYDRIN.



Which O-ring do I need for DICHLOROISOPROPYL ETHER?

FFKM O-rings are the best option for contact with DICHLOROISOPROPYL ETHER, based on chemical resistance and relative cost. These materials offer chemical resistance to DICHLOROISOPROPYL ETHER with a maximum swelling of less than 15%. AU, EPDM, FPM, FEP and FVMQ O-rings are less resistant to DICHLOROISOPROPYL ETHER and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ and PTFE O-rings for DICHLOROISOPROPYL ETHER, as these materials are not recommended or have not been tested for resistance to DICHLOROISOPROPYL ETHER.



Which O-ring do I need for DICHLOROMETHANE?

PTFE O-rings are the best option for contact with DICHLOROMETHANE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHLOROMETHANE with a maximum swelling of less than 15%, but at a higher cost than PTFE. FVMQ and FPM O-rings are less resistant to DICHLOROMETHANE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FEP and AU O-rings for DICHLOROMETHANE, as these materials are not recommended or have not been tested for resistance to DICHLOROMETHANE.



Which O-ring do I need for DICHLOROPHENOL?

FFKM O-rings are the best option for contact with DICHLOROPHENOL, based on chemical resistance and relative cost. These materials offer chemical resistance to DICHLOROPHENOL with a maximum swelling of less than 15%. NBR, HNBR, FPM, FVMQ and AU O-rings are less resistant to DICHLOROPHENOL and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DICHLOROPHENOL, as these materials are not recommended or have not been tested for resistance to DICHLOROPHENOL.



Which O-ring do I need for DICHLOROPHENOXYACETIC ACID?

FPM O-rings are the best option for contact with DICHLOROPHENOXYACETIC ACID, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHLOROPHENOXYACETIC ACID with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DICHLOROPHENOXYACETIC ACID and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DICHLOROPHENOXYACETIC ACID, as these materials are not recommended or have not been tested for resistance to DICHLOROPHENOXYACETIC ACID.



Which O-ring do I need for DICHLOROPROPANE?

FPM O-rings are the best option for contact with DICHLOROPROPANE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICHLOROPROPANE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DICHLOROPROPANE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DICHLOROPROPANE, as these materials are not recommended or have not been tested for resistance to DICHLOROPROPANE.



Which O-ring do I need for DICHLOROPROPENE?

FFKM O-rings are the best option for contact with DICHLOROPROPENE, based on chemical resistance and relative cost. These materials offer chemical resistance to DICHLOROPROPENE with a maximum swelling of less than 15%. NBR, HNBR, FPM, FVMQ and AU O-rings are less resistant to DICHLOROPROPENE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DICHLOROPROPENE, as these materials are not recommended or have not been tested for resistance to DICHLOROPROPENE.



Which O-ring do I need for DICYCLOHEXYLAMINE?

HNBR O-rings are the best option for contact with DICYCLOHEXYLAMINE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DICYCLOHEXYLAMINE with a maximum swelling of less than 15%, but at a higher cost than HNBR. VMQ, NBR and FEP O-rings are less resistant to DICYCLOHEXYLAMINE and should only be used after checking the application conditions. Do not use EPDM, FPM, FVMQ, AU and PTFE O-rings for DICYCLOHEXYLAMINE, as these materials are not recommended or have not been tested for resistance to DICYCLOHEXYLAMINE.



Which O-ring do I need for DICYCLOHEXYLAMMONIUM NITRATE?

EPDM O-rings are the best option for contact with DICYCLOHEXYLAMMONIUM NITRATE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DICYCLOHEXYLAMMONIUM NITRATE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR, HNBR and FPM O-rings are less resistant to DICYCLOHEXYLAMMONIUM NITRATE and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DICYCLOHEXYLAMMONIUM NITRATE, as these materials are not recommended or have not been tested for resistance to DICYCLOHEXYLAMMONIUM NITRATE.



Which O-ring do I need for DIELDRIN?

FFKM O-rings are the best option for contact with DIELDRIN, based on chemical resistance and relative cost. These materials offer chemical resistance to DIELDRIN with a maximum swelling of less than 15%. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIELDRIN and should only be used after checking the application conditions. Do not use EPDM, VMQ, FPM, FEP and PTFE O-rings for DIELDRIN, as these materials are not recommended or have not been tested for resistance to DIELDRIN.



Which O-ring do I need for DIESEL FUEL?

NBR O-rings are the best option for contact with DIESEL FUEL, based on chemical resistance and relative cost. HNBR, FPM, FVMQ, PTFE and FFKM O-rings offer the same chemical resistance to DIESEL FUEL with a maximum swelling of less than 15%, but at a higher cost than NBR. VMQ and AU O-rings are less resistant to DIESEL FUEL and should only be used after checking the application conditions. Do not use EPDM and FEP O-rings for DIESEL FUEL, as these materials are not recommended or have not been tested for resistance to DIESEL FUEL.



Which O-ring do I need for DIESEL OIL?

NBR O-rings are the best option for contact with DIESEL OIL, based on chemical resistance and relative cost. HNBR, FPM, FEP, FVMQ, PTFE and FFKM O-rings offer the same chemical resistance to DIESEL OIL with a maximum swelling of less than 15%, but at a higher cost than NBR. AU O-rings are less resistant to DIESEL OIL and should only be used after checking the application conditions. Do not use EPDM and VMQ O-rings for DIESEL OIL, as these materials are not recommended or have not been tested for resistance to DIESEL OIL.



Which O-ring do I need for DI-ESTER SYNTHETIC LUBRICANTS?

FPM O-rings and FEP O-rings are the best option for contact with DI-ESTER SYNTHETIC LUBRICANTS, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DI-ESTER SYNTHETIC LUBRICANTS with a maximum swelling of less than 15%, but at a higher cost than FPM and FEP. NBR, HNBR and FVMQ O-rings are less resistant to DI-ESTER SYNTHETIC LUBRICANTS and should only be used after checking the application conditions. Do not use EPDM, VMQ, AU and PTFE O-rings for DI-ESTER SYNTHETIC LUBRICANTS, as these materials are not recommended or have not been tested for resistance to DI-ESTER SYNTHETIC LUBRICANTS.



Which O-ring do I need for DIETHANOLAMINE?

EPDM O-rings are the best option for contact with DIETHANOLAMINE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIETHANOLAMINE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR, HNBR and FPM O-rings are less resistant to DIETHANOLAMINE and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DIETHANOLAMINE, as these materials are not recommended or have not been tested for resistance to DIETHANOLAMINE.



Which O-ring do I need for DIETHYL CARBONATE?

EPDM O-rings are the best option for contact with DIETHYL CARBONATE, based on chemical resistance and relative cost. FPM, FVMQ and FFKM O-rings offer the same chemical resistance to DIETHYL CARBONATE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR and HNBR O-rings are less resistant to DIETHYL CARBONATE and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DIETHYL CARBONATE, as these materials are not recommended or have not been tested for resistance to DIETHYL CARBONATE.



Which O-ring do I need for DIETHYL ETHER?

AU O-rings and PTFE O-rings are the best option for contact with DIETHYL ETHER, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIETHYL ETHER with a maximum swelling of less than 15%, but at a higher cost than AU and PTFE. FVMQ O-rings are less resistant to DIETHYL ETHER and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FPM and FEP O-rings for DIETHYL ETHER, as these materials are not recommended or have not been tested for resistance to DIETHYL ETHER.



Which O-ring do I need for DIETHYL PHTHALATE?

FPM O-rings are the best option for contact with DIETHYL PHTHALATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIETHYL PHTHALATE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIETHYL PHTHALATE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIETHYL PHTHALATE, as these materials are not recommended or have not been tested for resistance to DIETHYL PHTHALATE.



Which O-ring do I need for DIETHYL SEBACATE?

PTFE O-rings are the best option for contact with DIETHYL SEBACATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIETHYL SEBACATE with a maximum swelling of less than 15%, but at a higher cost than PTFE. EPDM, VMQ, FPM, FEP, FVMQ and HNBR O-rings are less resistant to DIETHYL SEBACATE and should only be used after checking the application conditions. Do not use NBR and AU O-rings for DIETHYL SEBACATE, as these materials are not recommended or have not been tested for resistance to DIETHYL SEBACATE.



Which O-ring do I need for DIETHYL SULFATE?

EPDM O-rings are the best option for contact with DIETHYL SULFATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIETHYL SULFATE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, FEP and FPM O-rings are less resistant to DIETHYL SULFATE and should only be used after checking the application conditions. Do not use NBR, HNBR, FVMQ, AU and PTFE O-rings for DIETHYL SULFATE, as these materials are not recommended or have not been tested for resistance to DIETHYL SULFATE.



Which O-ring do I need for DIETHYLAMINE?

PTFE O-rings are the best option for contact with DIETHYLAMINE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIETHYLAMINE with a maximum swelling of less than 15%, but at a higher cost than PTFE. NBR, EPDM, HNBR and VMQ O-rings are less resistant to DIETHYLAMINE and should only be used after checking the application conditions. Do not use FPM, FEP, FVMQ and AU O-rings for DIETHYLAMINE, as these materials are not recommended or have not been tested for resistance to DIETHYLAMINE.



Which O-ring do I need for DIETHYLANILINE?

EPDM O-rings are the best option for contact with DIETHYLANILINE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIETHYLANILINE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR, HNBR and FPM O-rings are less resistant to DIETHYLANILINE and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DIETHYLANILINE, as these materials are not recommended or have not been tested for resistance to DIETHYLANILINE.



Which O-ring do I need for DIETHYLBENZENE?

FPM O-rings are the best option for contact with DIETHYLBENZENE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIETHYLBENZENE with a maximum swelling of less than 15%, but at a higher cost than FPM. FEP and FVMQ O-rings are less resistant to DIETHYLBENZENE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, AU and PTFE O-rings for DIETHYLBENZENE, as these materials are not recommended or have not been tested for resistance to DIETHYLBENZENE.



Which O-ring do I need for DIETHYLENE GLYCOL?

NBR O-rings and EPDM O-rings are the best option for contact with DIETHYLENE GLYCOL, based on chemical resistance and relative cost. HNBR, FPM, FEP, FVMQ, PTFE and FFKM O-rings offer the same chemical resistance to DIETHYLENE GLYCOL with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. VMQ O-rings are less resistant to DIETHYLENE GLYCOL and should only be used after checking the application conditions. Do not use AU O-rings for DIETHYLENE GLYCOL, as these materials are not recommended or have not been tested for resistance to DIETHYLENE GLYCOL.



Which O-ring do I need for DIETHYLENE GLYCOL BUTYL ETHER?

EPDM O-rings are the best option for contact with DIETHYLENE GLYCOL BUTYL ETHER, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIETHYLENE GLYCOL BUTYL ETHER with a maximum swelling of less than 15%, but at a higher cost than EPDM. FEP and FPM O-rings are less resistant to DIETHYLENE GLYCOL BUTYL ETHER and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FVMQ, AU and PTFE O-rings for DIETHYLENE GLYCOL BUTYL ETHER, as these materials are not recommended or have not been tested for resistance to DIETHYLENE GLYCOL BUTYL ETHER.



Which O-ring do I need for DIETHYLHEXYL PHTHALATE?

FFKM O-rings are the best option for contact with DIETHYLHEXYL PHTHALATE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIETHYLHEXYL PHTHALATE with a maximum swelling of less than 15%. EPDM, FPM, FEP, FVMQ and VMQ O-rings are less resistant to DIETHYLHEXYL PHTHALATE and should only be used after checking the application conditions. Do not use NBR, HNBR, AU and PTFE O-rings for DIETHYLHEXYL PHTHALATE, as these materials are not recommended or have not been tested for resistance to DIETHYLHEXYL PHTHALATE.



Which O-ring do I need for DIETHYLHEXYL SEBACATE?

FPM O-rings and FEP O-rings are the best option for contact with DIETHYLHEXYL SEBACATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIETHYLHEXYL SEBACATE with a maximum swelling of less than 15%, but at a higher cost than FPM and FEP. EPDM, VMQ and FVMQ O-rings are less resistant to DIETHYLHEXYL SEBACATE and should only be used after checking the application conditions. Do not use NBR, HNBR, AU and PTFE O-rings for DIETHYLHEXYL SEBACATE, as these materials are not recommended or have not been tested for resistance to DIETHYLHEXYL SEBACATE.



Which O-ring do I need for DIFLUORODIBROMOMETHANE?

FFKM O-rings are the best option for contact with DIFLUORODIBROMOMETHANE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIFLUORODIBROMOMETHANE with a maximum swelling of less than 15%. EPDM and FEP O-rings are less resistant to DIFLUORODIBROMOMETHANE and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FPM, FVMQ, AU and PTFE O-rings for DIFLUORODIBROMOMETHANE, as these materials are not recommended or have not been tested for resistance to DIFLUORODIBROMOMETHANE.



Which O-ring do I need for DIFLUOROETHANE?

FFKM O-rings are the best option for contact with DIFLUOROETHANE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIFLUOROETHANE with a maximum swelling of less than 15%. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIFLUOROETHANE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FPM, FEP and PTFE O-rings for DIFLUOROETHANE, as these materials are not recommended or have not been tested for resistance to DIFLUOROETHANE.



Which O-ring do I need for DIFLUOROMONOCHLOROETHANE?

FPM O-rings are the best option for contact with DIFLUOROMONOCHLOROETHANE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIFLUOROMONOCHLOROETHANE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIFLUOROMONOCHLOROETHANE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIFLUOROMONOCHLOROETHANE, as these materials are not recommended or have not been tested for resistance to DIFLUOROMONOCHLOROETHANE.



Which O-ring do I need for DIGLYCOL CHLOROFORMATE?

EPDM O-rings are the best option for contact with DIGLYCOL CHLOROFORMATE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIGLYCOL CHLOROFORMATE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR, HNBR and FPM O-rings are less resistant to DIGLYCOL CHLOROFORMATE and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DIGLYCOL CHLOROFORMATE, as these materials are not recommended or have not been tested for resistance to DIGLYCOL CHLOROFORMATE.



Which O-ring do I need for DIGLYCOLIC ACID?

EPDM O-rings are the best option for contact with DIGLYCOLIC ACID, based on chemical resistance and relative cost. FPM, FVMQ, PTFE and FFKM O-rings offer the same chemical resistance to DIGLYCOLIC ACID with a maximum swelling of less than 15%, but at a higher cost than EPDM. NBR, HNBR and VMQ O-rings are less resistant to DIGLYCOLIC ACID and should only be used after checking the application conditions. Do not use FEP and AU O-rings for DIGLYCOLIC ACID, as these materials are not recommended or have not been tested for resistance to DIGLYCOLIC ACID.



Which O-ring do I need for DIHEXYL PHTHALATE?

PTFE O-rings are the best option for contact with DIHEXYL PHTHALATE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIHEXYL PHTHALATE with a maximum swelling of less than 15%. FFKM O-rings are less resistant to DIHEXYL PHTHALATE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FPM, FEP, FVMQ and AU O-rings for DIHEXYL PHTHALATE, as these materials are not recommended or have not been tested for resistance to DIHEXYL PHTHALATE.



Which O-ring do I need for DIHYDROXYDIPHENYLSULFONE?

EPDM O-rings are the best option for contact with DIHYDROXYDIPHENYLSULFONE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIHYDROXYDIPHENYLSULFONE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR, HNBR and FPM O-rings are less resistant to DIHYDROXYDIPHENYLSULFONE and should only be used after checking the application conditions. Do not use FEP, AU and PTFE O-rings for DIHYDROXYDIPHENYLSULFONE, as these materials are not recommended or have not been tested for resistance to DIHYDROXYDIPHENYLSULFONE.



Which O-ring do I need for DIISOBUTYL KETONE?

EPDM O-rings are the best option for contact with DIISOBUTYL KETONE, based on chemical resistance and relative cost. FEP, PTFE and FFKM O-rings offer the same chemical resistance to DIISOBUTYL KETONE with a maximum swelling of less than 15%, but at a higher cost than EPDM. Do not use NBR, HNBR, VMQ, FPM, FVMQ and AU O-rings for DIISOBUTYL KETONE, as these materials are not recommended or have not been tested for resistance to DIISOBUTYL KETONE.



Which O-ring do I need for DIISOBUTYLCARBINOL?

NBR O-rings are the best option for contact with DIISOBUTYLCARBINOL, based on chemical resistance and relative cost. HNBR, FPM, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DIISOBUTYLCARBINOL with a maximum swelling of less than 15%, but at a higher cost than NBR. VMQ O-rings are less resistant to DIISOBUTYLCARBINOL and should only be used after checking the application conditions. Do not use EPDM, FEP and PTFE O-rings for DIISOBUTYLCARBINOL, as these materials are not recommended or have not been tested for resistance to DIISOBUTYLCARBINOL.



Which O-ring do I need for DIISOBUTYLENE?

FPM O-rings are the best option for contact with DIISOBUTYLENE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIISOBUTYLENE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FEP and FVMQ O-rings are less resistant to DIISOBUTYLENE and should only be used after checking the application conditions. Do not use EPDM, VMQ, AU and PTFE O-rings for DIISOBUTYLENE, as these materials are not recommended or have not been tested for resistance to DIISOBUTYLENE.



Which O-ring do I need for DIISOOCTYL SEBACATE?

FFKM O-rings are the best option for contact with DIISOOCTYL SEBACATE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIISOOCTYL SEBACATE with a maximum swelling of less than 15%. FPM, FEP, NBR, EPDM, HNBR, VMQ and FVMQ O-rings are less resistant to DIISOOCTYL SEBACATE and should only be used after checking the application conditions. Do not use AU and PTFE O-rings for DIISOOCTYL SEBACATE, as these materials are not recommended or have not been tested for resistance to DIISOOCTYL SEBACATE.



Which O-ring do I need for DIISOPROPYL ETHER?

FPM O-rings are the best option for contact with DIISOPROPYL ETHER, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIISOPROPYL ETHER with a maximum swelling of less than 15%, but at a higher cost than FPM. Do not use NBR, EPDM, HNBR, VMQ, FEP, FVMQ, AU and PTFE O-rings for DIISOPROPYL ETHER, as these materials are not recommended or have not been tested for resistance to DIISOPROPYL ETHER.



Which O-ring do I need for DIISOPROPYL KETONE?

EPDM O-rings are the best option for contact with DIISOPROPYL KETONE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIISOPROPYL KETONE with a maximum swelling of less than 15%, but at a higher cost than EPDM. FEP O-rings are less resistant to DIISOPROPYL KETONE and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FPM, FVMQ, AU and PTFE O-rings for DIISOPROPYL KETONE, as these materials are not recommended or have not been tested for resistance to DIISOPROPYL KETONE.



Which O-ring do I need for DIISOPROPYLBENZENE?

FPM O-rings are the best option for contact with DIISOPROPYLBENZENE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIISOPROPYLBENZENE with a maximum swelling of less than 15%, but at a higher cost than FPM. HNBR, FVMQ and AU O-rings are less resistant to DIISOPROPYLBENZENE and should only be used after checking the application conditions. Do not use NBR, EPDM, VMQ, FEP and PTFE O-rings for DIISOPROPYLBENZENE, as these materials are not recommended or have not been tested for resistance to DIISOPROPYLBENZENE.



Which O-ring do I need for DIISOPROPYLIDENE ACETONE?

FFKM O-rings are the best option for contact with DIISOPROPYLIDENE ACETONE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIISOPROPYLIDENE ACETONE with a maximum swelling of less than 15%. HNBR, EPDM and AU O-rings are less resistant to DIISOPROPYLIDENE ACETONE and should only be used after checking the application conditions. Do not use NBR, VMQ, FPM, FEP, FVMQ and PTFE O-rings for DIISOPROPYLIDENE ACETONE, as these materials are not recommended or have not been tested for resistance to DIISOPROPYLIDENE ACETONE.



Which O-ring do I need for DIMETHYL ACETAMIDE?

EPDM O-rings are the best option for contact with DIMETHYL ACETAMIDE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIMETHYL ACETAMIDE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR and HNBR O-rings are less resistant to DIMETHYL ACETAMIDE and should only be used after checking the application conditions. Do not use FPM, FEP, AU and PTFE O-rings for DIMETHYL ACETAMIDE, as these materials are not recommended or have not been tested for resistance to DIMETHYL ACETAMIDE.



Which O-ring do I need for DIMETHYL ANILINE?

FFKM O-rings are the best option for contact with DIMETHYL ANILINE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIMETHYL ANILINE with a maximum swelling of less than 15%. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIMETHYL ANILINE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FPM, FEP and PTFE O-rings for DIMETHYL ANILINE, as these materials are not recommended or have not been tested for resistance to DIMETHYL ANILINE.



Which O-ring do I need for DIMETHYL DISULFIDE?

NBR O-rings are the best option for contact with DIMETHYL DISULFIDE, based on chemical resistance and relative cost. HNBR, FPM, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DIMETHYL DISULFIDE with a maximum swelling of less than 15%, but at a higher cost than NBR. VMQ O-rings are less resistant to DIMETHYL DISULFIDE and should only be used after checking the application conditions. Do not use EPDM, FEP and PTFE O-rings for DIMETHYL DISULFIDE, as these materials are not recommended or have not been tested for resistance to DIMETHYL DISULFIDE.



Which O-ring do I need for DIMETHYL ETHER?

VMQ O-rings are the best option for contact with DIMETHYL ETHER, based on chemical resistance and relative cost. FVMQ, PTFE and FFKM O-rings offer the same chemical resistance to DIMETHYL ETHER with a maximum swelling of less than 15%, but at a higher cost than VMQ. Do not use NBR, EPDM, HNBR, FPM, FEP and AU O-rings for DIMETHYL ETHER, as these materials are not recommended or have not been tested for resistance to DIMETHYL ETHER.



Which O-ring do I need for DIMETHYL FORMALDEHYDE?

EPDM O-rings are the best option for contact with DIMETHYL FORMALDEHYDE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIMETHYL FORMALDEHYDE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR and HNBR O-rings are less resistant to DIMETHYL FORMALDEHYDE and should only be used after checking the application conditions. Do not use FPM, FEP, AU and PTFE O-rings for DIMETHYL FORMALDEHYDE, as these materials are not recommended or have not been tested for resistance to DIMETHYL FORMALDEHYDE.



Which O-ring do I need for DIMETHYL FORMAMIDE?

PTFE O-rings are the best option for contact with DIMETHYL FORMAMIDE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIMETHYL FORMAMIDE with a maximum swelling of less than 15%, but at a higher cost than PTFE. EPDM, VMQ, NBR, HNBR and FEP O-rings are less resistant to DIMETHYL FORMAMIDE and should only be used after checking the application conditions. Do not use FPM, FVMQ and AU O-rings for DIMETHYL FORMAMIDE, as these materials are not recommended or have not been tested for resistance to DIMETHYL FORMAMIDE.



Which O-ring do I need for DIMETHYL HYDRAZINE?

EPDM O-rings are the best option for contact with DIMETHYL HYDRAZINE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIMETHYL HYDRAZINE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, NBR and HNBR O-rings are less resistant to DIMETHYL HYDRAZINE and should only be used after checking the application conditions. Do not use FPM, FEP, AU and PTFE O-rings for DIMETHYL HYDRAZINE, as these materials are not recommended or have not been tested for resistance to DIMETHYL HYDRAZINE.



Which O-ring do I need for DIMETHYL PHENYL CARBINOL?

FPM O-rings are the best option for contact with DIMETHYL PHENYL CARBINOL, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIMETHYL PHENYL CARBINOL with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIMETHYL PHENYL CARBINOL and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIMETHYL PHENYL CARBINOL, as these materials are not recommended or have not been tested for resistance to DIMETHYL PHENYL CARBINOL.



Which O-ring do I need for DIMETHYL PHENYL METHANOL?

FPM O-rings are the best option for contact with DIMETHYL PHENYL METHANOL, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIMETHYL PHENYL METHANOL with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIMETHYL PHENYL METHANOL and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIMETHYL PHENYL METHANOL, as these materials are not recommended or have not been tested for resistance to DIMETHYL PHENYL METHANOL.



Which O-ring do I need for DIMETHYL PHTHALATE?

PTFE O-rings are the best option for contact with DIMETHYL PHTHALATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIMETHYL PHTHALATE with a maximum swelling of less than 15%, but at a higher cost than PTFE. EPDM, FPM, FEP and FVMQ O-rings are less resistant to DIMETHYL PHTHALATE and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ and AU O-rings for DIMETHYL PHTHALATE, as these materials are not recommended or have not been tested for resistance to DIMETHYL PHTHALATE.



Which O-ring do I need for DIMETHYL SULFOXIDE?

EPDM O-rings are the best option for contact with DIMETHYL SULFOXIDE, based on chemical resistance and relative cost. FVMQ and FFKM O-rings offer the same chemical resistance to DIMETHYL SULFOXIDE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, FEP, NBR and HNBR O-rings are less resistant to DIMETHYL SULFOXIDE and should only be used after checking the application conditions. Do not use FPM, AU and PTFE O-rings for DIMETHYL SULFOXIDE, as these materials are not recommended or have not been tested for resistance to DIMETHYL SULFOXIDE.



Which O-ring do I need for DIMETHYL TEREPHTHALATE?

FFKM O-rings are the best option for contact with DIMETHYL TEREPHTHALATE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIMETHYL TEREPHTHALATE with a maximum swelling of less than 15%. NBR, HNBR, FPM, FVMQ and AU O-rings are less resistant to DIMETHYL TEREPHTHALATE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIMETHYL TEREPHTHALATE, as these materials are not recommended or have not been tested for resistance to DIMETHYL TEREPHTHALATE.



Which O-ring do I need for DIMETHYLAMINE?

EPDM O-rings are the best option for contact with DIMETHYLAMINE, based on chemical resistance and relative cost. PTFE O-rings offer the same chemical resistance to DIMETHYLAMINE with a maximum swelling of less than 15%, but at a higher cost than EPDM. VMQ, FEP, FFKM and AU O-rings are less resistant to DIMETHYLAMINE and should only be used after checking the application conditions. Do not use NBR, HNBR, FPM and FVMQ O-rings for DIMETHYLAMINE, as these materials are not recommended or have not been tested for resistance to DIMETHYLAMINE.



Which O-ring do I need for DIMETHYLANILINE?

FFKM O-rings are the best option for contact with DIMETHYLANILINE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIMETHYLANILINE with a maximum swelling of less than 15%. EPDM and NBR O-rings are less resistant to DIMETHYLANILINE and should only be used after checking the application conditions. Do not use HNBR, VMQ, FPM, FEP, FVMQ, AU and PTFE O-rings for DIMETHYLANILINE, as these materials are not recommended or have not been tested for resistance to DIMETHYLANILINE.



Which O-ring do I need for DIMETHYLETHER?

FFKM O-rings are the best option for contact with DIMETHYLETHER, based on chemical resistance and relative cost. These materials offer chemical resistance to DIMETHYLETHER with a maximum swelling of less than 15%. Do not use NBR, EPDM, HNBR, VMQ, FPM, FEP, FVMQ, AU and PTFE O-rings for DIMETHYLETHER, as these materials are not recommended or have not been tested for resistance to DIMETHYLETHER.



Which O-ring do I need for DINITROCHLOROBENZENE?

FPM O-rings are the best option for contact with DINITROCHLOROBENZENE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DINITROCHLOROBENZENE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DINITROCHLOROBENZENE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DINITROCHLOROBENZENE, as these materials are not recommended or have not been tested for resistance to DINITROCHLOROBENZENE.



Which O-ring do I need for DINITROGEN TETROXIDE?

No rating 1 O-ring material is listed for DINITROGEN TETROXIDE in this chemical resistance guide. FFKM O-rings are less resistant to DINITROGEN TETROXIDE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FPM, FEP, FVMQ, AU and PTFE O-rings for DINITROGEN TETROXIDE, as these materials are not recommended or have not been tested for resistance to DINITROGEN TETROXIDE.



Which O-ring do I need for DINITROTOLUENE?

FFKM O-rings are the best option for contact with DINITROTOLUENE, based on chemical resistance and relative cost. These materials offer chemical resistance to DINITROTOLUENE with a maximum swelling of less than 15%. Do not use NBR, EPDM, HNBR, VMQ, FPM, FEP, FVMQ, AU and PTFE O-rings for DINITROTOLUENE, as these materials are not recommended or have not been tested for resistance to DINITROTOLUENE.



Which O-ring do I need for DINONYL PHTALATE?

PTFE O-rings are the best option for contact with DINONYL PHTALATE, based on chemical resistance and relative cost. These materials offer chemical resistance to DINONYL PHTALATE with a maximum swelling of less than 15%. FFKM O-rings are less resistant to DINONYL PHTALATE and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, FPM, FEP, FVMQ and AU O-rings for DINONYL PHTALATE, as these materials are not recommended or have not been tested for resistance to DINONYL PHTALATE.



Which O-ring do I need for DIOCTYL PHTHALATE?

FPM O-rings and PTFE O-rings are the best option for contact with DIOCTYL PHTHALATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIOCTYL PHTHALATE with a maximum swelling of less than 15%, but at a higher cost than FPM and PTFE. EPDM, FEP, FVMQ and VMQ O-rings are less resistant to DIOCTYL PHTHALATE and should only be used after checking the application conditions. Do not use NBR, HNBR and AU O-rings for DIOCTYL PHTHALATE, as these materials are not recommended or have not been tested for resistance to DIOCTYL PHTHALATE.



Which O-ring do I need for DIOCTYL SEBACATE?

FPM O-rings and PTFE O-rings are the best option for contact with DIOCTYL SEBACATE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIOCTYL SEBACATE with a maximum swelling of less than 15%, but at a higher cost than FPM and PTFE. EPDM, FEP, AU, VMQ and FVMQ O-rings are less resistant to DIOCTYL SEBACATE and should only be used after checking the application conditions. Do not use NBR and HNBR O-rings for DIOCTYL SEBACATE, as these materials are not recommended or have not been tested for resistance to DIOCTYL SEBACATE.



Which O-ring do I need for DIOCTYLAMINE?

NBR O-rings are the best option for contact with DIOCTYLAMINE, based on chemical resistance and relative cost. HNBR, FPM, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DIOCTYLAMINE with a maximum swelling of less than 15%, but at a higher cost than NBR. VMQ O-rings are less resistant to DIOCTYLAMINE and should only be used after checking the application conditions. Do not use EPDM, FEP and PTFE O-rings for DIOCTYLAMINE, as these materials are not recommended or have not been tested for resistance to DIOCTYLAMINE.



Which O-ring do I need for DIOXANE?

PTFE O-rings are the best option for contact with DIOXANE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIOXANE with a maximum swelling of less than 15%, but at a higher cost than PTFE. EPDM O-rings are less resistant to DIOXANE and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FPM, FEP, FVMQ and AU O-rings for DIOXANE, as these materials are not recommended or have not been tested for resistance to DIOXANE.



Which O-ring do I need for DIOXOLANE?

FFKM O-rings are the best option for contact with DIOXOLANE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIOXOLANE with a maximum swelling of less than 15%. EPDM O-rings are less resistant to DIOXOLANE and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FPM, FEP, FVMQ, AU and PTFE O-rings for DIOXOLANE, as these materials are not recommended or have not been tested for resistance to DIOXOLANE.



Which O-ring do I need for DIPENTENE?

FPM O-rings and PTFE O-rings are the best option for contact with DIPENTENE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIPENTENE with a maximum swelling of less than 15%, but at a higher cost than FPM and PTFE. NBR, HNBR, FEP and FVMQ O-rings are less resistant to DIPENTENE and should only be used after checking the application conditions. Do not use EPDM, VMQ and AU O-rings for DIPENTENE, as these materials are not recommended or have not been tested for resistance to DIPENTENE.



Which O-ring do I need for DIPHENYL?

FPM O-rings and PTFE O-rings are the best option for contact with DIPHENYL, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIPHENYL with a maximum swelling of less than 15%, but at a higher cost than FPM and PTFE. FEP and FVMQ O-rings are less resistant to DIPHENYL and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ and AU O-rings for DIPHENYL, as these materials are not recommended or have not been tested for resistance to DIPHENYL.



Which O-ring do I need for DIPHENYL OXIDES?

FPM O-rings and PTFE O-rings are the best option for contact with DIPHENYL OXIDES, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DIPHENYL OXIDES with a maximum swelling of less than 15%, but at a higher cost than FPM and PTFE. FEP, FVMQ and VMQ O-rings are less resistant to DIPHENYL OXIDES and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR and AU O-rings for DIPHENYL OXIDES, as these materials are not recommended or have not been tested for resistance to DIPHENYL OXIDES.



Which O-ring do I need for DIPHENYLAMINE?

FFKM O-rings are the best option for contact with DIPHENYLAMINE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIPHENYLAMINE with a maximum swelling of less than 15%. NBR, HNBR, FVMQ and AU O-rings are less resistant to DIPHENYLAMINE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FPM, FEP and PTFE O-rings for DIPHENYLAMINE, as these materials are not recommended or have not been tested for resistance to DIPHENYLAMINE.



Which O-ring do I need for DIPHENYLPROPANE?

FFKM O-rings are the best option for contact with DIPHENYLPROPANE, based on chemical resistance and relative cost. These materials offer chemical resistance to DIPHENYLPROPANE with a maximum swelling of less than 15%. NBR, HNBR, FPM, FVMQ and AU O-rings are less resistant to DIPHENYLPROPANE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DIPHENYLPROPANE, as these materials are not recommended or have not been tested for resistance to DIPHENYLPROPANE.



Which O-ring do I need for DISILANE?

FFKM O-rings are the best option for contact with DISILANE, based on chemical resistance and relative cost. These materials offer chemical resistance to DISILANE with a maximum swelling of less than 15%. Do not use NBR, EPDM, HNBR, VMQ, FPM, FEP, FVMQ, AU and PTFE O-rings for DISILANE, as these materials are not recommended or have not been tested for resistance to DISILANE.



Which O-ring do I need for DODECYLBENZENE?

FPM O-rings are the best option for contact with DODECYLBENZENE, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DODECYLBENZENE with a maximum swelling of less than 15%, but at a higher cost than FPM. NBR, HNBR, FVMQ and AU O-rings are less resistant to DODECYLBENZENE and should only be used after checking the application conditions. Do not use EPDM, VMQ, FEP and PTFE O-rings for DODECYLBENZENE, as these materials are not recommended or have not been tested for resistance to DODECYLBENZENE.



Which O-ring do I need for DOW CHEMICAL 50-4?

EPDM O-rings are the best option for contact with DOW CHEMICAL 50-4, based on chemical resistance and relative cost. These materials offer chemical resistance to DOW CHEMICAL 50-4 with a maximum swelling of less than 15%. FFKM, NBR and HNBR O-rings are less resistant to DOW CHEMICAL 50-4 and should only be used after checking the application conditions. Do not use VMQ, FPM, FEP, FVMQ, AU and PTFE O-rings for DOW CHEMICAL 50-4, as these materials are not recommended or have not been tested for resistance to DOW CHEMICAL 50-4.



Which O-ring do I need for DOW CHEMICAL ET378?

No rating 1 O-ring material is listed for DOW CHEMICAL ET378 in this chemical resistance guide. AU, FFKM, EPDM, FPM and FEP O-rings are less resistant to DOW CHEMICAL ET378 and should only be used after checking the application conditions. Do not use NBR, HNBR, VMQ, FVMQ and PTFE O-rings for DOW CHEMICAL ET378, as these materials are not recommended or have not been tested for resistance to DOW CHEMICAL ET378.



Which O-ring do I need for DOW CHEMICAL ET588?

EPDM O-rings are the best option for contact with DOW CHEMICAL ET588, based on chemical resistance and relative cost. These materials offer chemical resistance to DOW CHEMICAL ET588 with a maximum swelling of less than 15%. FFKM, NBR and HNBR O-rings are less resistant to DOW CHEMICAL ET588 and should only be used after checking the application conditions. Do not use VMQ, FPM, FEP, FVMQ, AU and PTFE O-rings for DOW CHEMICAL ET588, as these materials are not recommended or have not been tested for resistance to DOW CHEMICAL ET588.



Which O-ring do I need for DOW CORNING 11?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 11, based on chemical resistance and relative cost. FPM, FEP, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 11 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. HNBR and VMQ O-rings are less resistant to DOW CORNING 11 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 11, as these materials are not recommended or have not been tested for resistance to DOW CORNING 11.



Which O-ring do I need for DOW CORNING 1208, 4050, 6620, F-60, XF-60?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 1208, 4050, 6620, F-60, XF-60, based on chemical resistance and relative cost. HNBR, VMQ, FPM, FEP and FFKM O-rings offer the same chemical resistance to DOW CORNING 1208, 4050, 6620, F-60, XF-60 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. Do not use FVMQ, AU and PTFE O-rings for DOW CORNING 1208, 4050, 6620, F-60, XF-60, as these materials are not recommended or have not been tested for resistance to DOW CORNING 1208, 4050, 6620, F-60, XF-60.



Which O-ring do I need for DOW CORNING 1265 FLUOROSILICONE FLUID?

EPDM O-rings are the best option for contact with DOW CORNING 1265 FLUOROSILICONE FLUID, based on chemical resistance and relative cost. VMQ, FPM, FEP, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 1265 FLUOROSILICONE FLUID with a maximum swelling of less than 15%, but at a higher cost than EPDM. NBR, HNBR and FVMQ O-rings are less resistant to DOW CORNING 1265 FLUOROSILICONE FLUID and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 1265 FLUOROSILICONE FLUID, as these materials are not recommended or have not been tested for resistance to DOW CORNING 1265 FLUOROSILICONE FLUID.



Which O-ring do I need for DOW CORNING 200?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 200, based on chemical resistance and relative cost. FPM, FEP, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 200 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. HNBR, FVMQ and VMQ O-rings are less resistant to DOW CORNING 200 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 200, as these materials are not recommended or have not been tested for resistance to DOW CORNING 200.



Which O-ring do I need for DOW CORNING 220?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 220, based on chemical resistance and relative cost. HNBR, FPM, FEP and FFKM O-rings offer the same chemical resistance to DOW CORNING 220 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. Do not use VMQ, FVMQ, AU and PTFE O-rings for DOW CORNING 220, as these materials are not recommended or have not been tested for resistance to DOW CORNING 220.



Which O-ring do I need for DOW CORNING 3?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 3, based on chemical resistance and relative cost. FPM, FEP, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 3 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. HNBR and VMQ O-rings are less resistant to DOW CORNING 3 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 3, as these materials are not recommended or have not been tested for resistance to DOW CORNING 3.



Which O-ring do I need for DOW CORNING 33?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 33, based on chemical resistance and relative cost. FPM, FEP, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 33 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. HNBR, FVMQ and VMQ O-rings are less resistant to DOW CORNING 33 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 33, as these materials are not recommended or have not been tested for resistance to DOW CORNING 33.



Which O-ring do I need for DOW CORNING 4?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 4, based on chemical resistance and relative cost. FPM, FEP, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 4 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. HNBR and VMQ O-rings are less resistant to DOW CORNING 4 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 4, as these materials are not recommended or have not been tested for resistance to DOW CORNING 4.



Which O-ring do I need for DOW CORNING 44?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 44, based on chemical resistance and relative cost. FPM, FEP, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 44 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. HNBR, FVMQ and VMQ O-rings are less resistant to DOW CORNING 44 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 44, as these materials are not recommended or have not been tested for resistance to DOW CORNING 44.



Which O-ring do I need for DOW CORNING 5?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 5, based on chemical resistance and relative cost. FPM, FEP, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 5 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. HNBR, FVMQ and VMQ O-rings are less resistant to DOW CORNING 5 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 5, as these materials are not recommended or have not been tested for resistance to DOW CORNING 5.



Which O-ring do I need for DOW CORNING 510?

EPDM O-rings are the best option for contact with DOW CORNING 510, based on chemical resistance and relative cost. FPM, FEP, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 510 with a maximum swelling of less than 15%, but at a higher cost than EPDM. NBR, HNBR, FVMQ and VMQ O-rings are less resistant to DOW CORNING 510 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 510, as these materials are not recommended or have not been tested for resistance to DOW CORNING 510.



Which O-ring do I need for DOW CORNING 55?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 55, based on chemical resistance and relative cost. FPM, FEP, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 55 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. HNBR, FVMQ and VMQ O-rings are less resistant to DOW CORNING 55 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 55, as these materials are not recommended or have not been tested for resistance to DOW CORNING 55.



Which O-ring do I need for DOW CORNING 550?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING 550, based on chemical resistance and relative cost. HNBR, FPM, FEP, AU, PTFE and FFKM O-rings offer the same chemical resistance to DOW CORNING 550 with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. FVMQ and VMQ O-rings are less resistant to DOW CORNING 550 and should only be used after checking the application conditions.



Which O-ring do I need for DOW CORNING 704?

EPDM O-rings are the best option for contact with DOW CORNING 704, based on chemical resistance and relative cost. FPM, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 704 with a maximum swelling of less than 15%, but at a higher cost than EPDM. NBR, HNBR, FVMQ and VMQ O-rings are less resistant to DOW CORNING 704 and should only be used after checking the application conditions. Do not use FEP and PTFE O-rings for DOW CORNING 704, as these materials are not recommended or have not been tested for resistance to DOW CORNING 704.



Which O-ring do I need for DOW CORNING 705?

EPDM O-rings are the best option for contact with DOW CORNING 705, based on chemical resistance and relative cost. FPM, FEP, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 705 with a maximum swelling of less than 15%, but at a higher cost than EPDM. NBR, HNBR, FVMQ and VMQ O-rings are less resistant to DOW CORNING 705 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 705, as these materials are not recommended or have not been tested for resistance to DOW CORNING 705.



Which O-ring do I need for DOW CORNING 710?

EPDM O-rings are the best option for contact with DOW CORNING 710, based on chemical resistance and relative cost. FPM, FEP, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING 710 with a maximum swelling of less than 15%, but at a higher cost than EPDM. NBR, HNBR, FVMQ and VMQ O-rings are less resistant to DOW CORNING 710 and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW CORNING 710, as these materials are not recommended or have not been tested for resistance to DOW CORNING 710.



Which O-ring do I need for DOW CORNING F-60 FLUID?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING F-60 FLUID, based on chemical resistance and relative cost. HNBR, FPM, FEP, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING F-60 FLUID with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. Do not use VMQ and PTFE O-rings for DOW CORNING F-60 FLUID, as these materials are not recommended or have not been tested for resistance to DOW CORNING F-60 FLUID.



Which O-ring do I need for DOW CORNING F-61 FLUID?

NBR O-rings and EPDM O-rings are the best option for contact with DOW CORNING F-61 FLUID, based on chemical resistance and relative cost. HNBR, FPM, FEP, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DOW CORNING F-61 FLUID with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. Do not use VMQ and PTFE O-rings for DOW CORNING F-61 FLUID, as these materials are not recommended or have not been tested for resistance to DOW CORNING F-61 FLUID.



Which O-ring do I need for DOW GUARD?

NBR O-rings and EPDM O-rings are the best option for contact with DOW GUARD, based on chemical resistance and relative cost. HNBR, VMQ, FPM, FEP, FVMQ and FFKM O-rings offer the same chemical resistance to DOW GUARD with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. AU O-rings are less resistant to DOW GUARD and should only be used after checking the application conditions. Do not use PTFE O-rings for DOW GUARD, as these materials are not recommended or have not been tested for resistance to DOW GUARD.



Which O-ring do I need for DOWTHERM 209?

EPDM O-rings are the best option for contact with DOWTHERM 209, based on chemical resistance and relative cost. FPM, FEP and FFKM O-rings offer the same chemical resistance to DOWTHERM 209 with a maximum swelling of less than 15%, but at a higher cost than EPDM. NBR, HNBR, VMQ and FVMQ O-rings are less resistant to DOWTHERM 209 and should only be used after checking the application conditions. Do not use AU and PTFE O-rings for DOWTHERM 209, as these materials are not recommended or have not been tested for resistance to DOWTHERM 209.



Which O-ring do I need for DOWTHERM A?

FPM O-rings and PTFE O-rings are the best option for contact with DOWTHERM A, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DOWTHERM A with a maximum swelling of less than 15%, but at a higher cost than FPM and PTFE. FEP and FVMQ O-rings are less resistant to DOWTHERM A and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ and AU O-rings for DOWTHERM A, as these materials are not recommended or have not been tested for resistance to DOWTHERM A.



Which O-ring do I need for DOWTHERM E?

FPM O-rings and FEP O-rings are the best option for contact with DOWTHERM E, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DOWTHERM E with a maximum swelling of less than 15%, but at a higher cost than FPM and FEP. FVMQ O-rings are less resistant to DOWTHERM E and should only be used after checking the application conditions. Do not use NBR, EPDM, HNBR, VMQ, AU and PTFE O-rings for DOWTHERM E, as these materials are not recommended or have not been tested for resistance to DOWTHERM E.



Which O-ring do I need for DRINKING WATER?

NBR O-rings and EPDM O-rings are the best option for contact with DRINKING WATER, based on chemical resistance and relative cost. HNBR, VMQ, FPM, FEP, FVMQ and FFKM O-rings offer the same chemical resistance to DRINKING WATER with a maximum swelling of less than 15%, but at a higher cost than NBR and EPDM. Do not use AU and PTFE O-rings for DRINKING WATER, as these materials are not recommended or have not been tested for resistance to DRINKING WATER.



Which O-ring do I need for DRY CLEANING FLUIDS?

FPM O-rings are the best option for contact with DRY CLEANING FLUIDS, based on chemical resistance and relative cost. These materials offer chemical resistance to DRY CLEANING FLUIDS with a maximum swelling of less than 15%. FVMQ, FFKM, NBR, HNBR and FEP O-rings are less resistant to DRY CLEANING FLUIDS and should only be used after checking the application conditions. Do not use EPDM, VMQ, AU and PTFE O-rings for DRY CLEANING FLUIDS, as these materials are not recommended or have not been tested for resistance to DRY CLEANING FLUIDS.



Which O-ring do I need for DTE 20 SERIES?

FPM O-rings and AU O-rings are the best option for contact with DTE 20 SERIES, based on chemical resistance and relative cost. FFKM O-rings offer the same chemical resistance to DTE 20 SERIES with a maximum swelling of less than 15%, but at a higher cost than FPM and AU. NBR, HNBR, FEP and FVMQ O-rings are less resistant to DTE 20 SERIES and should only be used after checking the application conditions. Do not use EPDM, VMQ and PTFE O-rings for DTE 20 SERIES, as these materials are not recommended or have not been tested for resistance to DTE 20 SERIES.



Which O-ring do I need for DTE LIGHT OIL?

NBR O-rings are the best option for contact with DTE LIGHT OIL, based on chemical resistance and relative cost. HNBR, FPM, FEP, FVMQ, AU and FFKM O-rings offer the same chemical resistance to DTE LIGHT OIL with a maximum swelling of less than 15%, but at a higher cost than NBR. VMQ O-rings are less resistant to DTE LIGHT OIL and should only be used after checking the application conditions. Do not use EPDM and PTFE O-rings for DTE LIGHT OIL, as these materials are not recommended or have not been tested for resistance to DTE LIGHT OIL.



Contact us

               All items marked with a * are required.